OK, I picked up fresh flux and more fuel for the torch. This is a micro torch.
I figured out that part of my problem was that I was using a silver braze and not silver solder which melts at a much lower temp. About 450F compared to 1350F. I picked up a roll of silver solder this time.
Got home, popped things apart, cleaned off the epoxy, fluxed things up, clamped things together like they were supposed to wind up so everything was aligned properly, and proceeded to solder. The instant the solder flowed, it stuck EVERYTHING together. It bonded the templates together and only stuck the templates to one side of the hemostat.
I finally wound up tinning the hemostat jaws, clamping things together, adding a drop of flux and then heating until the solder just flowed from the hemostat to the template.
That worked pretty well, but one set of templates warped a touch. No problem, I’ll just bend them back. Popped the solder joint with little or no effort. It popped easier than the epoxy did. At least I had to apply a fair amount of heat to get the epoxy to let loose.
On top of all of that, the resulting burners are UGLY with a capital YUCK! I couldn’t polish anything out and with all the silver solder mess, they are just plain ugly. Functional, but ugly.
One set is soldered. I ain’t messing with the other two. If I make another set, I will probably get the aluminum brazing stuff I saw and try that. It melts at about 1100F, should flow a tad easier than the silver braze, and be considerably stronger than the silver solder.
If anyone else is considering making a set of these, I certainly recommend the epoxy over the silver solder.