Quote Originally Posted by hardhat View Post
ACE Hardware is the place. Give them a try as I purchased a bunch there recently.
Yep, Ace hardware is the place I stared at all the labels for over half an hour. They must've had 8 or 9 different brands and types. All of it a bit confusing that's why I backed off and went with my usual slow dry.

It just struck me that the 5-minute had a higher bond strength. I figure the slow dry will eventually be phased out as everyone wants the quick stuff. More research will always be done on the stuff people want and a profit can be made.

Let's hope a chemist can chime in and explain all this to us.